Nickel Sulfide Flotation: Recovering Pentlandite

Key takeaways
- Nickel sulfide ore is concentrated by flotation before smelting, because smelting raw ore would be uneconomic.
- Pentlandite is the main nickel mineral; pyrrhotite is the main problem.
- Pyrrhotite depression is the core of the circuit design, because pyrrhotite dilutes concentrate and consumes smelter capacity.
- Grind size and pH control decide whether pentlandite is liberated and whether the pyrrhotite stays down.
- Magnetic separation and regrinding can improve concentrate grade when pyrrhotite is magnetic or locked.
Nickel sulfide ore is a flotation success story. The nickel sits in pentlandite, a sulfide mineral that responds well to xanthate collectors, and the gangue is mostly silicates that do not. A well-designed circuit can upgrade ore grading around 1% Ni to a concentrate of 8–15% Ni, which is economic to smelt.
The difficulty is not floating pentlandite. It is keeping pyrrhotite out of the concentrate. Pyrrhotite is an iron sulfide that carries little or no nickel, but it floats readily and can report to the concentrate along with pentlandite. Every tonne of pyrrhotite in the concentrate is a tonne of smelter capacity spent on waste.
The minerals and the deposit
Magmatic sulfide deposits form when sulfide liquid separates from silicate magma and concentrates nickel, copper and platinum-group elements. The main nickel mineral is pentlandite, usually accompanied by pyrrhotite, chalcopyrite and magnetite. The ore texture ranges from massive sulfide to disseminated blebs in silicate rock.
Massive ore is easy to liberate but can be abrasive and dense. Disseminated ore requires finer grinding to release the pentlandite from silicates. The deposit’s texture therefore sets the grind size, the circuit arrangement and the expected recovery.
Grinding and liberation
Pentlandite is usually liberated at a P80 of roughly 75–150 µm, but the exact target depends on the ore. Fine dissemination may need 50–75 µm; coarse blebs may be liberated at 150 µm. Overgrinding is a particular risk because serpentine and talc minerals in the gangue produce slimes that coat bubbles, increase reagent consumption and stabilise froth that is hard to control.
The pyrrhotite problem
Pyrrhotite has no fixed composition; it ranges from FeS to Fe7S8, and its flotation behaviour changes with iron deficiency and oxidation. Some pyrrhotite is naturally floatable, some is depressed by lime, and some becomes floatable again after oxidation. That variability is what makes nickel flotation difficult.
The standard approach is to raise the pH with lime and use a depressant such as guar gum or sodium sulfite to keep pyrrhotite down. The dosage has to be tuned to the ore; too little and pyrrhotite reports to the concentrate, too much and pentlandite recovery falls. The circuit often includes a regrind of the rougher concentrate to liberate locked particles before cleaning.
Circuit design
- Crush and grind. Reduce the ore to the liberation size, usually P80 75–150 µm, in a rod or ball mill with a classifier.
- Rougher flotation. Float pentlandite and pyrrhotite together with xanthate at pH 9–11. The rougher should maximise nickel recovery, even if the concentrate is low grade.
- Regrind and clean. Regrind the rougher concentrate to liberate locked particles, then clean at a higher pH with depressant to reject pyrrhotite.
- Magnetic separation (optional). Pyrrhotite is magnetic, while pentlandite is not. A magnetic separation or gravity step can remove pyrrhotite from the cleaner concentrate.
- Dewater and smelt. Thicken and filter the concentrate to a moisture suitable for smelting or shipping.
| Parameter | Typical range | Effect |
|---|---|---|
| Grind size | P80 75–150 µm | Liberation of pentlandite from silicates and pyrrhotite |
| pH | 9–11 | Lime depresses pyrrhotite and pyrite |
| Collector | Xanthate, 20–80 g/t | Floats pentlandite and pyrrhotite |
| Depressant | Guar, sodium sulfite, or lime | Reduces pyrrhotite flotation |
| Concentrate grade | 8–15% Ni | Smelter feed specification |
Bulk versus selective flotation
Nickel circuits are usually described as bulk or selective. A bulk circuit floats pentlandite and pyrrhotite together, then relies on regrinding and cleaning to reject pyrrhotite. A selective circuit tries to depress pyrrhotite in the rougher, producing a higher-grade concentrate at the cost of nickel recovery.
The right choice depends on the ore and the smelter. A smelter that can handle a lower-grade concentrate may prefer a bulk circuit with high nickel recovery. A smelter with tight limits on magnesium and sulphur may require a cleaner concentrate, even if recovery falls. The circuit should be designed around the smelter contract, not just the mill’s recovery target.
Smelting and concentrate specification
Nickel concentrate is smelted to matte, then refined to nickel metal or converted to other products. The smelter cares about nickel grade, sulphur, iron, magnesium and penalty elements. Magnesium is particularly important because it raises slag viscosity and can limit the smelter’s throughput.
The concentrator therefore has two customers: the smelter and the mine. A concentrate that meets the smelter specification but loses too much nickel is not good; neither is one that recovers every particle but contains too much pyrrhotite. The economic optimum is a concentrate grade and recovery that maximise value across the chain.
Operating control
Nickel flotation is controlled on grind size, pH, reagent dosage and froth depth. The most important measurement is the concentrate grade and the pyrrhotite content, because small changes in depressant dose can shift the balance between recovery and grade. Online assay systems, where available, help operators respond before a shift’s production is lost.
Water quality also matters. Recycled process water can carry residual depressant, xanthate and dissolved salts, which change flotation behaviour. A circuit that performs well with fresh water may need dose adjustments when the plant moves to a closed water balance.
The reagent scheme
A typical nickel sulfide circuit uses xanthate as the collector, a frother such as MIBC, lime for pH control and a depressant for pyrrhotite and gangue. The reagent scheme is often developed in laboratory tests and then refined on site, because the ore’s response changes with oxidation, grind size and water chemistry.
Guar gum is a common pyrrhotite depressant, but it also affects pentlandite if overdosed. Sodium sulfite can help by modifying pyrrhotite surfaces, and lime raises pH and precipitates metal ions that might activate unwanted minerals. The combination is ore-specific, and a scheme that works at one mine may fail at another.
Commissioning and ramp-up
Nickel flotation plants often take longer to ramp up than expected. The first ore is rarely the same as the metallurgical sample, and the circuit has to be tuned to the actual feed. A commissioning plan should include a period of flexible operation, with the ability to adjust grind, pH and reagent doses without stopping production.
It also helps to have a metallurgist on site during ramp-up, not just a control-room operator. Nickel flotation is sensitive enough that small changes in froth appearance, pulp density or reagent addition can shift the result. The earlier those signals are recognised, the faster the plant reaches design performance.
What goes wrong
Talc and serpentine are common gangue minerals in nickel sulfide deposits. They float naturally, produce a stable froth and dilute the concentrate. CMC or a similar depressant is often needed to keep them down. The problem is worse when the ore is weathered or when the grind is too fine.
Oxidation is another issue. Sulfide minerals oxidise in stockpiles and in the mill, and oxidised surfaces do not respond to xanthate. A circuit that performs well on fresh ore can lose recovery on ore that has been stockpiled for months. Blending fresh and oxidised ore, or adding a sulfidising agent, can help.

For the processing context, see our pages on nickel processing and the flotation equipment category.
Rule of thumb: if the concentrate grade is low and the nickel recovery is high, the problem is probably pyrrhotite or talc, not liberation. Check the depressant dose and the grind before adding more flotation capacity.
Frequently asked questions
What mineral carries nickel in sulfide ore?
Pentlandite, a nickel-iron sulfide with the approximate formula (Fe,Ni)9S8. It is usually accompanied by pyrrhotite, chalcopyrite and magnetite.
Why is pyrrhotite a problem in nickel flotation?
Pyrrhotite is an iron sulfide that floats readily but carries little nickel. It dilutes the concentrate, consumes smelter capacity and raises transport costs, so the circuit must depress it.
What pH is used for nickel sulfide flotation?
Usually pH 9–11, raised with lime. The lime helps depress pyrrhotite and pyrite, but the optimum depends on the ore and the depressant scheme.
Can magnetic separation help nickel flotation?
Sometimes. Pyrrhotite is magnetic and pentlandite is not, so a magnetic separation step can remove pyrrhotite from the cleaner concentrate. It is most useful when pyrrhotite is strongly magnetic and well liberated.
What causes low nickel recovery in flotation?
Common causes are insufficient liberation, oxidised sulfide surfaces, talc or serpentine slimes, and excessive depressant. A grind and mineralogy check is the first step.
Troubleshooting a nickel flotation circuit? Send us your grind, reagent scheme and concentrate assays and we will review the selectivity.
Talk to a Jinhao engineer